Variations – 5.5ml-2830ml, Rectangle & Square Alumina Crucible
Code | Outer Dim(L×W×H) | Wall Thickness | Capacity | Material | ID of Compatible Furnace |
---|---|---|---|---|---|
AC3201 | 50×20×10mm | 2mm | 5.5ml | 99% Alumina | >24mm |
AC3202 | 100×10×10mm | 1.5mm | 5.5ml | 99% Alumina | >13mm |
AC3203 | 75×18×14mm | 2mm | 10ml | 99% Alumina | >22mm |
AC3204 | 60×30×15mm | 3mm | 16ml | 99% Alumina | >35mm |
AC3205 | 50×25×23mm | 2mm | 20ml | 99% Alumina | >30mm |
AC3206 | 50×25×35mm | 3mm | 26ml | 99% Alumina | >30mm |
AC3207 | 60×40×20mm | 3mm | 30ml | 99% Alumina | >43mm |
AC3208 | 120×30×15mm | 2.5mm | 35ml | 99% Alumina | >35mm |
AC3209 | 100×100×25mm | 4mm | 150ml | 99% Alumina | >105mm |
AC3210 | 120×60×40mm | 5mm | 190ml | 99% Alumina | >65mm |
AC3211 | 85×80×40mm | 4mm | 195ml | 99% Alumina | >85mm |
AC3212 | 90×60×45mm | 3mm | 200ml | 99% Alumina | >65mm |
AC3213 | 120×80×30mm | 4mm | 205ml | 99% Alumina | >85mm |
AC3214 | 85×85×40mm | 4mm | 210ml | 99% Alumina | >90mm |
AC3215 | 125×83×40mm | 5mm | 290ml | 99% Alumina | >86mm |
AC3216 | 200×100×25mm | 4mm | 370ml | 99% Alumina | >105mm |
AC3217 | 200×100×50mm | 4mm | 800ml | 99% Alumina | >105mm |
AC3218 | 305×90×60mm | 6mm | 1100ml | 99% Alumina | >96mm |
AC3219 | 200×200×50mm | 7mm | 1480ml | 99% Alumina | >208mm |
AC3220 | 250×155×80mm | 7mm | 2400ml | 99% Alumina | >160mm |
AC3221 | 300×180×70mm | 8mm | 2830ml | 99% Alumina | >185mm |
À LIRE IMPÉRATIVEMENT avant de commander
Avis sur les dimensions du creuset
Il existe une grande différence de dimensions du creuset d'alumine entre avant et après la cuisson.
Si vous êtes particulier avec la taille du creuset, veuillez nous contacter pour vous fournir les dimensions réelles du creuset qui vous intéresse.
À SAVOIR après réception
- Please bake the crucible in the oven at 105℃ for 120 minutes to remove moisture content before the first use.
- DO NOT use open flame or direct heating equipment to heat the crucible, please make sure to use box muffle furnace with temperature control system.
- DO NOT heat up or cool down too fast, The temperature change below 1200℃ should be less than 5℃/ min, and the temperature change above 1200℃ should be less than 4℃/ min.
- When cooling the crucible, it is recommended to turn on the temperature control to cool down. Turning off the power at high temperature may lead to product cracking if the cooling speed is too fast in the early cooling stage.
- La distance entre le produit et l'élément chauffant (tel qu'un tube de carbone, une tige de silicium-molybdène ou un fil chauffant, etc.) doit être> 5cm.
- Le fond du grand creuset ne doit pas entrer en contact direct avec le fond du four. Il est suggéré d'utiliser un tampon en caoutchouc corindon ou d'autres matériaux résistants à la température pour soulever le creuset (comme indiqué sur l'image de droite) pour former une convection d'air et prolonger la durée de vie du creuset.